FrescoJet(TM) Process Adhesion Evaluated by Independent Lab
Wednesday, February 25, 2009 at 09:48PM In the course of qualifying our FrescoJet process for their application, one of our customers sent samples of the process performed on glass to an independent laboratory to have adhesion tests performed.
We are pleased to share the results from the test:
They indicate that on glass, without FrescoJet, our UV digital printing was achieving approximately 0 pounds-per-square inch of holding strength.
With FrescoJet, adhesion increased to an astonishing 25 pounds-per-square inch.
Hopefully this technology will allow us to bring UV digital printing to previously impossible uses!
Guy Newcomer | Comments Off | 